Caractérisation de la corrosivité des frigoporteurs.

Zur Beurteilung der Korrosivität von Kühlsolen.

Auteurs : JAUNICH H., REINHARD G., KOCH R. K., et al.

Type d'article : Article

Résumé

Coolants in technical cooling plants have to maintain usually temperatures under 0 °C. However, the characterization of their corrosivity on the basis of ASTM D 1384 is carried out at temperatures above 70 °C. It is shown that formiate contained salt coolants which have, in general, a sufficient cooling effect, will be degraded already more and more at temperatures above 40 °C with formation of corrosion promoting species. Therefore, it is proposed to modify this test method according to the really existing conditions in cooling plants.

Détails

  • Titre original : Zur Beurteilung der Korrosivität von Kühlsolen.
  • Identifiant de la fiche : 2000-2536
  • Langues : Allemand
  • Sujet : Réglementation
  • Source : KI Luft Kältetech. - n. 4
  • Date d'édition : 04/2000
  • Document disponible en consultation à la bibliothèque du siège de l'IIF uniquement.

Liens


Voir d'autres articles du même numéro (10)
Voir la source