Deuxième comparaison VAMAS sur la mesure des pertes en courant alternatif : mesure par magnétisation des pertes hystérétiques dans des brins multifilamentaires de niobium-titane.

Second VAMAS alternating-current loss measurement intercomparison: magnetization measurement of low-frequency (hysteretic) alternating-current loss in niobium-titanium multifilamentary strands.

Auteurs : COLLINGS E. W., SUMPTION M. D., ITOH K., WADA H., TACHIKAWA K.

Type d'article : Article

Résumé

Two sets of multifilamentary niobium-titanium strands were subjected to interlaboratory testing: 1) copper matrix, filament diameters: 0.5, 1, 3, and 12 micrometers; 2) cupronickel matrix, filament diameters: 0.4, 0.5, and 1 micrometer. In the light of all the results, factors contributing to alternating-current loss error are discussed and recommendations are made concerning the specification of future alternating-current loss measurement intercomparisons.

Détails

  • Titre original : Second VAMAS alternating-current loss measurement intercomparison: magnetization measurement of low-frequency (hysteretic) alternating-current loss in niobium-titanium multifilamentary strands.
  • Identifiant de la fiche : 1998-0748
  • Langues : Anglais
  • Source : Cryogenics - vol. 37 - n. 1
  • Date d'édition : 01/1997

Liens


Voir d'autres articles du même numéro (2)
Voir la source