Document IIF

Maîtrise de la température de Curie (Tc) par hydrogénation dans du La(Fe0.88Si0.12)13 formé par frittage flash ("spark plasma sintering," SPS).

Control of Curie temperature (Tc) with hydrogenation in La(Fe0.88Si0.12)13 shaped by spark plasma sintering (SPS).

Numéro : 1621

Auteurs : FUJINAKA T., WATANABE N., FUJITA A., et al.

Résumé

The purpose of this investigation is maintenance of the original shape of La(Fe0.88Si0.12)13Hy sintered bulk specimen after hydrogenation for intentional control of the Curie temperature(Tc). Homogenized La(Fe0.88Si0.12)13 powder could be molded into a bulk form with leaving pores in the range of 1 to 10 vol. % by controlling temperature of the spark plasma sintering (SPS). The plate with thickness of 0.4mm which was made from the bulk maintained its original shape after hydrogenation, while Tc was controlled.

Documents disponibles

Format PDF

Pages : 2 p.

Disponible

  • Prix public

    10 €

  • Prix membre*

    7,50 €

* meilleur tarif applicable selon le type d'adhésion (voir le détail des avantages des adhésions individuelles et collectives)

Détails

  • Titre original : Control of Curie temperature (Tc) with hydrogenation in La(Fe0.88Si0.12)13 shaped by spark plasma sintering (SPS).
  • Identifiant de la fiche : 30012946
  • Langues : Anglais
  • Source : 6th International Conference on Magnetic Refrigeration at Room Temperature (Thermag VI). Proceedings: Victoria, Canada, September 7-10, 2014.
  • Date d'édition : 07/09/2014

Liens


Voir d'autres communications du même compte rendu (78)
Voir le compte rendu de la conférence