EQUIPMENT FOR LONG TERM CREEP TESTING AT CRYOGENIC TEMPERATURES.
Author(s) : YEN C. T.
Type of article: Article
Summary
EQUIPMENT AND PROCEDURES FOR LONG TERM CRYOGENIC CREEP TESTING ARE PRESENTED IN DETAIL. PARTICULAR ATTENTION WAS GIVEN TO THE MAINTAINING OF CONSTANT CRYOGENIC TEST TEMPERATURE AND WITH RESPECT TO THE STABILITY AND SENSITIVITY OF STRAIN MEASUREMENTS. TYPICAL LONG TERM CRYOGENIC CREEP TESTING RESULTS ON OXYGEN FREE HIGH CONDUCTIVITY COPPER ARE PRESENTED.
Details
- Original title: EQUIPMENT FOR LONG TERM CREEP TESTING AT CRYOGENIC TEMPERATURES.
- Record ID : 1985-0890
- Languages: English
- Source: Cryogenics - vol. 24 - n. 8
- Publication date: 1984
Links
See other articles in this issue (9)
See the source
-
A SIMPLIFIED METHOD FOR CHARPY IMPACT TESTING N...
- Author(s) : OGATA T.
- Date : 1982
- Languages : English
- Source: Cryogenics - vol. 22 - n. 9
View record
-
SPECIMEN TEMPERATURE RISE AND TESTING CONDITION...
- Author(s) : OGATA T.
- Date : 1991
- Languages : Japanese
- Source: Cryogenics/ Cryog. Eng. - vol. 26 - n. 3
View record
-
TEMPERATURE RISE DURING THE TENSILE TEST IN SUP...
- Author(s) : OGATA T.
- Date : 1985
- Languages : English
- Source: Cryogenics - vol. 25 - n. 8
View record
-
Shear strength testing of solid oxygen.
- Author(s) : BATES S. C., ALTSHULER T. L.
- Date : 1995/09
- Languages : English
- Source: Cryogenics - vol. 35 - n. 9
View record
-
4 K FRACTURE TOUGHNESS INVESTIGATIONS OF 316 LN...
- Author(s) : NYILAS A., YANAGI H.
- Date : 1989
- Languages : English
- Source: Cryogenics - vol. 29 - n. 3
View record